Stress corrosion cracking in October 2018 led to pipeline rupture near Prince George

(Files by Brendan Pawliw-MyPGNow)

The Transportation Safety Board has unveiled its report outlining the Enbridge Pipeline rupture and fire near Prince George in October in 2018.

The organization found that stress corrosion cracking led to the rupture resulting in the blaze.

Deficiencies in predicting the extent of the cracking and a deferred inspection led to a hazard being undetected prior to the rupture according to the TSB.

Following the rupture, the natural gas being transported was released and ignited.

No injuries were reported but 125 residents within a two-kilometre radius were evacuated.

In February of 2019, the Lheidli T’enneh filed a lawsuit against Enbridge following the pipeline burst.

The host first nation claims inadequate communication and the lack of emergency response from Enbridge were two of the main reasons behind the lawsuit.

In December, it was announced that the Enbridge West Coast Pipeline is operating at full capacity.

Something going on in the Cariboo you think people should know about?
Send us a news tip by emailing [email protected].

Continue Reading

ckbx Now playing play

cffm Now playing play

ckcq Now playing play

- Advertisement -

Related Articles

- Advertisement -

Latest News

Perscribed burns scheduled in the Siwash area

The BC Wildfire Service and Cariboo Chilcotin Natural Resource District will be conducting two prescribed burns in the Siwash area, 100 kms west of Williams Lake, starting on October 14 and continuing until October 24.

Williams Lake Community Forest opens 2026 project applications

Grant Applications for the Williams Lake Community Forest are now available for 2026 projects until 4 pm on Nov. 4.

100 Mile District General’s ER closed all day

Interior Health is cautioning residents in 100 Mile House and the surrounding area that the Emergency Room services will be unavailable today from 6 am until 7 pm on October 11.

[Content Warning] Two in hospital following car crash in South Quesnel

A car crash on Highway 97 in South Quesnel sees two people sent to the hospital with major injuries.

Unemployment on the rise in the Cariboo region

The year over year unemployment rate in the Cariboo was up substantially last month.
- Advertisement -